NYLON 6/6 EXTRUDED HEX
Extruded Nylon 6/6 offers a combination of good mechanical properties and excellent bearing and wear resistance. Its fatigue resistance, noise damping ability, corrosion resistance, light weight, and machinability make extruded nylon ideal for metal replacement applications, such as bearings, gears, sheaves, and sprockets. Compared to cast Nylon 6, Nylon 6/6 has a higher melting point, better mechanical properties due to greater hardness, and lower water absorption.
Mechanical Properties | |
---|---|
Tensile Stength | 12,000 |
Tensile Elongation | 25 |
Tensile Modulus | 350,000 |
Izod Impact Strength | 1.1 |
Flexural Strength | 15,500 |
Flexural Modulus | 440,000 |
Compressive Strength | 5,000 |
Compressive Modulus | |
Dynamic Coefficient of Friction | 0.26 |
Thermal Properties | |
---|---|
Heat Deflection Temperature at 66 PSI | 455 |
Heat Deflection Temperature at 264 PSI | 194 |
Maximum Serving Temperature for Short Term | 300 |
Maximum Serving Temperature for Long Term | 185 |
Thermal Conductivity | 1.7 |
Coefficient of Linear Thermal Expansion | 4.50 x 10^5 |
Flammability Rating | V-2 |
Electric/Physical Properties | |
---|---|
Volume Resistivity | 10^15 |
Surface Resistivity | |
Dielectric Strength | 350 |
Specific Gravity | 1.14 |
Toughness | M90 |
Rockwell Hardness Shore D | |
Water Absorption | 1.2 |